Toilet making process
Filter out large particle impurities, heavy metals and bacteria, etc.
-
Raw material mixing
Firstly, Mix the wonderful clay with water and cement in the mixing blunger.
-
Blanking
Cast the slip in the moulds and turn around the moulds so that the slip can fill every corner.
-
Porcelain body modifying
Check and modify the wet bodies, dry them. Check and dry bodies and smooth the surface.
-
Glazing
The effect of spraying glaze to the surface of body by spraying glaze sprayer is smooth and smooth.
-
Firing
Products after glazing will be carried to our kilns for firing. The temperature is up to 1280℃. After 12 hours of firing they have 6 hours of cooling.
-
QC
100% products inspection for each item.

86-13902798139